Casting

Draft angle calculator for castings

Get the minimum draft angle for your metal, mold type and internal or external surface, plus the draft per face and total widening in mm for a given mold depth. Unlocked with Pro.

What draft does

Vertical walls get a slight taper so the pattern draws cleanly from the sand, or the casting releases from a permanent mold. With too little draft the pattern or casting clings to the mold, and in a permanent mold the casting can seize. How much you need depends on the metal, the molding method, and whether the face is internal or external.

What you choose

  • Metal / alloy: gray iron (GG25), ductile iron (GGG40), cast steel, aluminum alloy, copper / bronze / brass, Zamak, magnesium alloy
  • Mold type: hand-rammed sand, machine-molded sand, permanent mold (die), shell mold
  • Surface type: external or internal (pockets, blind holes)
  • Mold depth (mm)

The result

Draft per face tells you, in millimeters, how much the wall moves from bottom to top, so you can check it against the drawing tolerance on the spot. A quick-reference table on the screen lists external and internal draft for five metals in sand molds.

  • Minimum draft angle (degrees)
  • Draft on one face (mm)
  • Total widening over both faces (mm)
  • Mold depth

Notes from the shop floor

The field notes explain why hand-rammed molds need more draft, what to do if you have to go below the minimum (mold coating, graphite or a core), how fast cooling in permanent molds affects release, and how to finish with a draft analysis in your CAD software. An info box suggests extra draft for rough surfaces.

Without Pro you see the input form and the formula; the angle, the draft amounts and the note details unlock with Pro. If the customer drawing or your company standard calls for a different angle, that wins.

Frequently asked questions

What draft angle should a casting have?

There is no single number; the metal, the molding method, and whether the face is internal or external all change it. The app gives the minimum angle for your combination and asks for more draft on internal faces than on external ones.

How much does draft change the part dimensions?

The deeper the mold, the bigger the difference between the bottom and top of a wall. The app gives the draft per face and the total widening over both faces in millimeters.

Why are permanent molds less forgiving on draft?

Metal molds cool the casting fast, so it is more likely to grip the die. A field note in the app advises never going under the table values in permanent molds, and going above the minimum for cast steel and ductile iron.

You may also need

All calculators and features →