Casting

Gating system calculator for castings

From total metal weight, pouring time and sprue height, get sprue, runner and ingate cross-sections, metal velocity and a turbulence warning. Unlocked with Pro.

What the gating system controls

Sprue, runner and ingate sections decide how fast and how calmly metal enters the mold. Fast, turbulent flow drags oxide and gas into the casting and erodes the mold. This calculator sizes all three in one pass and checks the metal velocity straight away.

What goes in

Pouring time is your input; the field notes explain how it is usually estimated on the shop floor. Switch to US inch units in Settings and weight is asked in ounces, height in inches.

  • Metal / alloy: eight options, each showing the density used in the calculation
  • Gating system type: pressurized, balanced, unpressurized, and a dedicated aluminum option; the section ratio is printed on each entry
  • Total metal weight, casting plus gating (g)
  • Pouring time (s)
  • Sprue height (cm)

What comes out

  • Sprue cross-section (cm²)
  • Sprue diameter for a round sprue (cm)
  • Runner cross-section (cm²)
  • Ingate cross-section (cm²)
  • Flow rate (cm³/s)
  • Metal velocity (cm/s)

The velocity check

The calculated velocity is compared with a limit for the metal group: one for aluminum, another for iron, steel and bronze. Below the limit you get an OK, close to it a caution, and above it a turbulence-risk warning that suggests lowering the sprue height or enlarging the section.

Without Pro the input form and formula stay visible; the sections, the velocity check and the field-note details open with Pro. Treat the numbers as preliminary sizing and confirm them by watching the first pours and the quality of the castings.

Frequently asked questions

How do you calculate sprue size?

Metal weight and density give the volume, and pouring time turns that into a flow rate. Sprue height gives the metal velocity; the sprue section follows from flow rate and velocity, and the runner and ingate follow the ratio of the system you picked.

What is the difference between a pressurized and an unpressurized gating system?

In a pressurized system the smallest section is at the ingate, so metal enters fast and turbulence is more likely. In an unpressurized system the choke is at the sprue, the metal slows down, and oxide entrainment drops.

Why is aluminum gated differently?

Aluminum grows an oxide skin almost instantly. A generous ingate keeps velocity low so that skin is less likely to break up and end up in the casting; the app has a separate system option and velocity limit for aluminum.

You may also need

All calculators and features →