Plastic injection

Venting calculator for injection molds

Trapped air is a common cause of burn marks and short shots. Enter part volume to see how many vents you need, the total vent area and a vent depth suited to your material.

Where does the air go?

As melt enters the cavity, it pushes the air ahead of it. If the air has nowhere to go, it compresses, heats up and burns the plastic, or the last corner of the cavity never fills. The first reflex in many shops is to raise pressure, but the real problem is often the venting.

MoldBench's venting calculator works out from the part volume how much vent area you need and turns that into a vent count. Available with Pro.

Useful before you calculate

The top of the screen earns its keep before you've entered a single value.

  • A reference table of vent depth, width and land by material group
  • Location guidance: the last point to fill, the tips of deep ribs, remote corners and pockets
  • A guideline on how often to place vents relative to surface area
  • The vent depth range and material group for the resin you select

Inputs and results

  • Input: material (PP, HDPE, LDPE, PS, ABS, PC, PA6, PA66, PVC, POM, PMMA, PET)
  • Input: part wall thickness (mm)
  • Input: estimated part volume (mm³)
  • Result: recommended vent count
  • Result: total vent area (mm²)
  • Result: default vent width (mm) and the mid value of vent depth (mm)

On the shop floor

The field notes cover the practical side. Trapped air gets extremely hot as it's compressed and scorches the material; in deep ribs and narrow pockets this diesel effect is a major risk. A vent that's too deep flashes, one that's too shallow won't let the air out, so start from the table and fine-grind to size. Besides parting-line vents, ejector pin clearances and core inserts can serve as air paths. Porous sintered steel inserts offer a permanent fix in critical spots. Vents clog in production and need regular cleaning.

Treat the recommended count as a starting point, and fine-tune the vents on the tool based on burn marks and fill during the first trials.

Frequently asked questions

How deep should vents be in an injection mold?

It depends on the material: too deep and it flashes, too shallow and the air stays in. The app shows the depth range for your material's group and puts the mid value in the result.

How many vents do I need?

The app works out the total vent area from the part volume and turns it into a recommended vent count using the default vent width. The location guidance on the screen tells you where to put them.

What causes burn marks on molded parts?

Usually trapped air: with nowhere to escape, it compresses, heats up and scorches the plastic. A field note in the app tells you to check the vents before you raise injection pressure.

You may also need